A-A-59962
3.2.2 Reinforcement material. The material shall contain a high solids polymer face coating for
protection against abrasion. The maximum weight shall be 20.0 ounces per square yard when
tested in accordance with ASTM D3776. The maximum thermal shrinkage in either direction
shall be 1.0 percent when tested in accordance with NFPA 1971. The maximum vertical
flammability shall be no more than 1 second after flame and a maximum char length of 1.0 inch
when tested in accordance with ASTM D6413/D6413M.
4. REGULATORY REQUIREMENTS. The offeror/contractor is encouraged to use recovered
materials to the maximum extent practicable, in accordance with paragraph 23.403 of the Federal
Acquisition Regulation (FAR).
5. PRODUCT CONFORMANCE PROVISIONS.
5.1 Product conformance. The products provided shall meet the salient characteristics of this
CID, conform to the producer's own drawings, specifications, standards, and quality assurance
practices, and be the same product offered for sale in the commercial marketplace. The
government reserves the right to require proof of such conformance.
6. PACKAGING. Preservation, packing, and marking shall be as specified in the contract or
order.
7. NOTES.
7.1 Source of documents.
7.1.1 ASTM. ASTM standards are available from ASTM International at www.astm.org.
7.1.2 NFPA. National Fire Protection Association (NFPA) standards are available from NFPA
at www.nfpa.org.
7.1.3 FAR. The Federal Acquisition Regulation may be obtained from the Superintendent of
Documents, U.S. Government Printing Office at www.acquisition.gov/far.
7.2 Figures. The photos contained in this CID are only for reference purposes.
3
For Parts Inquires call Parts Hangar, Inc (727) 493-0744